ADC12 vs A380: How to Choose Between Two Common Die Casting Alloys

ADC12 vs A380: How to Choose Between Two Common Die Casting Alloys

  • Post author:
  • Post category:Blog

ADC12 vs A380 is one of the most common questions in an aluminum die casting RFQ. A drawing from a US or European design team often calls out A380. A supplier in Japan, China or Southeast Asia usually runs ADC12 every day. The two alloys are close, but they are not identical, and the difference matters when a buyer has to approve a substitution.

This article compares the two alloys on composition, castability and performance, and explains what to check before accepting one in place of the other.

Where Each Alloy Comes From

Both alloys belong to the aluminum-silicon-copper family, the workhorse group for high-pressure die casting.

  • ADC12 is defined in the Japanese standard JIS H 5302. It is the default die casting alloy across Japan and much of Asia.
  • A380 is defined in the US standard ASTM B85. It is the default alloy in most North American drawings.

Because supply chains follow these standards, the alloy a factory stocks often depends more on its region than on the part. That is why the substitution question comes up so often.

ADC12 vs A380: Composition Compared

The main differences are silicon and copper:

  • Silicon: ADC12 is specified at 9.6–12.0%, A380 at 7.5–9.5%.
  • Copper: ADC12 is specified at 1.5–3.5%, A380 at 3.0–4.0%.
  • Impurity limits: the two standards also set different maximums for elements such as zinc and iron, which matters for recycled-alloy supply.

By composition, ADC12 actually sits closer to A383 (ASTM B85) than to A380. In Europe, the nearest family is EN AC-46000 / AlSi9Cu3(Fe) under EN 1706. Buyers searching for an ADC12 equivalent will see all of these names. The full JIS composition table is published in Yamaha Motor’s JIS data sheet for aluminium alloy die castings.

What the Difference Means in Production

Castability. Higher silicon improves fluidity. ADC12 fills thin walls, deep ribs and fine fins more easily and is less prone to hot cracking. That is one reason it dominates electronics housings and other thin-walled parts.

Strength and ductility. A380’s higher copper and lower silicon generally give it slightly better tensile strength and elongation. For most housings and covers the gap is small. For parts with high load, impact or fatigue requirements, it should be checked against the drawing, not assumed.

Corrosion. Both alloys contain copper, so neither is a strong performer bare in outdoor or salt environments. In practice, the surface treatment (chromate conversion, powder coat or paint) does most of the work for both.

Machining and finishing. Both machine well. Neither is a good choice for decorative anodizing; the high silicon content gives a grey, uneven finish. If a part needs a cosmetic anodized surface, the alloy question has to be reopened at the design stage.

Can ADC12 Replace A380 on Your Drawing?

Often, yes, but the decision belongs to the customer’s engineering team, not the supplier. A sound substitution review covers four points:

  1. Mechanical requirements. Compare the drawing’s minimum strength or elongation, if any, with the typical values of the proposed alloy.
  2. Pressure tightness. If the part must hold air, gas or liquid, confirm the leak test method. Porosity control and impregnation matter more here than the alloy itself (see how to control porosity with production parameters).
  3. Finish and coating. Check that the specified coating has been qualified on the proposed alloy.
  4. Documentation. Agree on how the alloy will be verified, for example by spectro analysis of each lot, and record the change formally. For automotive parts, that means a deviation or PPAP update, not an email.

The same logic applies when a part moves from machined billet to die casting. 6061 or 7075 billet cannot be die cast, so the alloy changes completely. We covered that case in die casting robot housings.

How EKO Handles Alloy Selection

At EKO, alloy choice is reviewed during DFM, before the tool is designed. Our plants in Penang and Kedah, Malaysia run aluminum die casting from 125T to 800T and zinc die casting on hot-chamber and multi-slide machines. Alloy composition can be verified on our in-house spectro analyzer, and pressure-tight parts can be impregnated. For a broader overview of alloy options, including zinc, see the difference between aluminium and zinc alloys.

FAQ

Is ADC12 the same as A380? No. They are close relatives in the Al-Si-Cu family, but ADC12 has more silicon and less copper. By composition, ADC12 is closer to A383.

What is the ADC12 equivalent in the US and Europe? In the US, A383 is the closest match, and A380 is often accepted as a practical substitute. In Europe, the EN AC-46000 / AlSi9Cu3(Fe) family is the usual cross-reference.

Which is stronger, ADC12 or A380? A380 generally shows slightly higher strength and elongation. ADC12 casts thin walls more easily. For most housings the difference is small, but parts with specified mechanical values should be checked against the drawing.

If you are reviewing an alloy callout on a new or transferred part, we welcome a conversation with your engineering or sourcing team through our contact page.